• Titàn Strip ak Materyèl Foil:Pi Titàn (CP) ak FOIL alyaj Titàn,Klas 1, Klas 2, Klas 5, Klas 5, Klas 7 ak Klas 9
• Fòm: Bann sèl, nan bobin, oswa sou bobin.Sèvis tranche ki disponib
• Dimansyon:Epesè: ≥0.01mm: 20~1000mm, Longè: Kòm demann lan
• Kondisyon:Woule frèt (Y) ~ Woule cho (R) ~ Annealed (M) ~ Estati solid
• Estanda:ASTM B265, AMS 4911, AMS 4902, ASTM F67, ASTM F136 elatriye
• Aplikasyon:Elektwonik, pwodui chimik, mont, linèt, bijou, machandiz espòtif, machin, ekipman plating, ekipman anviwònman, gòlf ak endistri machin presizyon.
Titàn Alliages Materyèl Non komen | ||
Gr1 | UNS R50250 | CP-Ti |
Gr2 | UNS R50400 | CP-Ti |
Gr4 | UNS R50700 | CP-Ti |
Gr7 | UNS R52400 | Ti-0.20Pd |
G9 | UNS R56320 | Ti-3AL-2.5V |
G11 | UNS R52250 | Ti-0.15Pd |
G12 | UNS R53400 | Ti-0.3Mo-0.8Ni |
G16 | UNS R52402 | Ti-0.05Pd |
G23 | UNS R56407 | Ti-6Al-4V ELI |
Titàn bann ak FOIL:Nou sitou bay pi bon kalite Titàn Strip nan Gr1, Gr2, Gr4 klas;Pou Foil alyaj Titàn, Nou sitou bay Gr5, Gr7, Gr9, Gr11, Gr12, Gr16, Gr23 ak lòt klas, Yo pwodui sou baz plak Titàn ak plis woule frèt;pwosesis pwodiksyon an nan fèy Titàn se pi konplike.Kontwòl la deformation se pi estrikteman nan pwosesis la nan woule.Sa ka koupe nan diferan gwosè selon bezwen kliyan an, anpil diminye tan an nan livrezon.
Klas | Konpozisyon chimik, pousan pwa (%) | ||||||||||||
C (≤) | O (≤) | N (≤) | H (≤) | Fe (≤) | Al | V | Pd | Ru | Ni | Mo | Lòt Eleman Max.chak | Lòt Eleman Max.total | |
Gr1 | 0.08 | 0.18 | 0.03 | 0.015 | 0.20 | — | — | — | — | — | — | 0.1 | 0.4 |
Gr2 | 0.08 | 0.25 | 0.03 | 0.015 | 0.30 | — | — | — | — | — | — | 0.1 | 0.4 |
Gr4 | 0.08 | 0.25 | 0.03 | 0.015 | 0.30 | — | — | — | — | — | — | 0.1 | 0.4 |
Gr5 | 0.08 | 0.20 | 0.05 | 0.015 | 0.40 | 5.56.75 | 3.5 4.5 | — | — | — | — | 0.1 | 0.4 |
Gr7 | 0.08 | 0.25 | 0.03 | 0.015 | 0.30 | — | — | 0.12 0.25 | — | 0.12 0.25 | — | 0.1 | 0.4 |
Gr9 | 0.08 | 0.15 | 0.03 | 0.015 | 0.25 | 2.5 3.5 | 2.0 3.0 | — | — | — | — | 0.1 | 0.4 |
Gr11 | 0.08 | 0.18 | 0.03 | 0.15 | 0.2 | — | — | 0.12 0.25 | — | — | — | 0.1 | 0.4 |
Gr12 | 0.08 | 0.25 | 0.03 | 0.15 | 0.3 | — | — | — | — | 0.6 0.9 | 0.2 0.4 | 0.1 | 0.4 |
Gr16 | 0.08 | 0.25 | 0.03 | 0.15 | 0.3 | — | — | 0.04 0.08 | — | — | — | 0.1 | 0.4 |
Gr23 | 0.08 | 0.13 | 0.03 | 0.125 | 0.25 | 5.5 6.5 | 3.5 4.5 | — | — | — | — | 0.1 | 0.1 |
Klas | Pwopriyete fizik | |||||||
Fòs rupture Min | Sede fòsMin (0.2%, konpanse) | Elongasyon nan 4D Min (%) | Rediksyon nan zòn Min (%) | Tès koube (reyon mandrin) | ||||
ksi | MPa | ksi | MPa | <1.8mm Nan epesè | 1.8-4.8mm nan epesè | |||
Gr1 | 35 | 240 | 20 | 138 | 24 | 30 | 1.5T | 2.0T |
Gr2 | 50 | 345 | 40 | 275 | 20 | 30 | 2.0T | 2.5T |
Gr4 | 80 | 550 | 70 | 483 | 15 | 25 | 2.5T | 3.0T |
Gr5 | 130 | 895 | 120 | 828 | 10 | 25 | 4.5T | 5.0T |
Gr7 | 50 | 345 | 40 | 275 | 20 | 30 | 2.0T | 2.5T |
Gr9 | 90 | 620 | 70 | 483 | 15 | 25 | 2.5T | 3.0T |
Gr11 | 35 | 240 | 20 | 138 | 24 | 30 | 1.5T | 2.0T |
Gr12 | 70 | 483 | 50 | 345 | 18 | 25 | 2.0T | 2.5T |
Gr16 | 50 | 345 | 40 | 275 | 20 | 30 | 2.0T | 2.5T |
Gr23 | 120 | 828 | 110 | 759 | 10 | 15 | 4.5T | 5.0T |
•Klas 1: Pi Titàn, relativman ba fòs ak segondè duktilite.
•Klas 2: pi Titàn ki pi itilize.Pi bon konbinezon de fòs
•Klas 3: Titàn segondè fòs, yo itilize pou plak Matris nan echanjeur chalè koki ak tib
•Klas 5: alyaj Titàn ki pi fabrike.Trè wo fòs.segondè rezistans chalè.
•Klas 7: Siperyè rezistans korozyon nan anviwònman diminye ak oksidasyon.
•Klas 9: Trè wo fòs ak rezistans korozyon.
•Klas 12: Pi bon rezistans chalè pase Titàn pi.Aplikasyon pou klas 7yèm ak 11yèm ane.
•Klas 23: Titàn-6Aluminium-4Vanadium ELI (Siplemantè Low Interstitial) Alloy pou aplikasyon chirijikal implant.